This particular filament (Sunlu matte HS PETG) is one of the absolute worst I’ve ever used WRT being hygroscopic. It arrived so wet that I had literal steam from the extruder the first time I wanted to use it. It took almost 48h in my drier to dry it completely so I could use it. Its been sitting in an airtight box with dessicant for 5 weeks and I needed to dry it for >16h for it to be usable again. The wet part in this print was in the bowden tube between dryer and printer, I restarted the print after took this image.

Sure it prints well at 300mm/s, but it is by no means matte at the temperatures that allow printing it at high speeds, it is actually very glossy. A huge bummer.

smooth first layer…so nice smooth first layer...so nice

  • MrQuallzin@lemmy.world
    link
    fedilink
    English
    arrow-up
    7
    ·
    17 days ago

    Why do I feel like I live in a perfect little world where my years old filament prints just fine without any special treatment… Sitting here at 45% humidity in the very wet pacific northwest and my PETG prints just fine. I’ve never understood it

    • ExcessShiv@lemmy.dbzer0.comOP
      link
      fedilink
      English
      arrow-up
      5
      ·
      edit-2
      17 days ago

      This is the only PETG I’ve ever had this issue with, normally I can just store them with dessicant and it’s fine.

      Right now RH is fairly low around 30-40% because it’s cold and winter, summer its usually around 60-80% here.